Nd:Ce:YAG - Neodymium, Cerium Co-doped Yttrium Aluminum Garnet

In double doped Nd:Ce:YAG crystals Cerium are chosen as sensitizer for Nd3+ ions because of its strong absorption in UV spectral region and efficient energy transfer to the Nd3+ excited state.

Keyword:

Nd:Ce:YAG flash lamp pumping energy transfer thermal distortion double doped

Nd:Ce:YAG - Neodymium, Cerium Co-doped Yttrium Aluminum Garnet

Category:

  • Description
  • Cas'Tech Class
  • Parameters
  • Introduction

    In double doped Nd:Ce:YAG crystals, Cerium are chosen as sensitizer for Nd3+ ions because of its strong absorption in UV spectral region at flash lamp pumping and efficient energy transfer to the Nd3+ excited state. As a result - thermal distortion in Nd:Ce:YAG is appreciably less and the output laser energy is greater than that in Nd:YAG at the same pumping. Therefore it is possible or realize high power lasers with good beam quality. Lasing wavelength at 1064 nm, laser damage threshold and thermal conductivity of the Nd:Ce:YAG crystals are the same as for Nd:YAG.

     

    CASTECH's laser crystal Nd:Ce:YAG is featured by

    •   High efficiency
    •   Low threshold
    •   Good anti-violet radiation property
    •   Good thermal stability
    •   High optical quality

      

    Table 1. Basic Properties
    Laser Transition4I3/2→4I11/2
    Laser Wavelength1.064 µm
    Photon Energy1.86×10-19 J @1.064 µm
    Emission Linewidth4.5 Å @1.064 µm
    Emission Cross Section (Nd 1 at.%)2.7~8.8 × 10-19 cm2
    Fluorescence Lifetime (Nd 1 at.%)230 µs
    Refractive Index1.8197 @1.064 µm

     

    Table 2. Specifications
    Dopant ConcentrationNd: 1.1~1.4 at.%,  Ce: 0.05~0.1 at.%
    Rod Sizes

    Diameter: 3~6 mm, Length: 40~80 mm;

    Upon request of customer

    Dimensional Tolerances

    Diameter: ±0.1mm 

    Length: ±0.5 mm

    Surface Quality (Scratch/Dig)10/5 to MIL-PRF-13830B
    Wavefront Distortionλ/4 @633 nm
    Flatness λ/8 @633 nm
    Parallelism≦30 arc sec
    Perpendicularity≦15 arc min
    Chamfer≦0.2 mm×45°
    AR Coating≦0.2% @1064 nm

     

     

    Key words: