CASTECH
Nd:YLF - Neodymium Doped Yttrium Lithium Fluoride
+
  • Nd:YLF - Neodymium Doped Yttrium Lithium Fluoride

Nd:YLF - Neodymium Doped Yttrium Lithium Fluoride

CASTECH grows Nd:YLF using Czochralski method with high quality starting materials for crystal growth. We inspect the whole boules with interferometry and their scattering particles with He-Ne laser.

Keyword:

laser crystal Nd:YLF rod Czochralski method Nd-doped laser-active material

Nd:YLF - Neodymium Doped Yttrium Lithium Fluoride

Category:

  • Description
  • Cas'Tech Class
  • Parameters
  • Introduction

    CASTECH grows Nd:YLF crystals using Czochralski method. The use of high quality starting materials for crystal growth, whole boule interferometry, and precise inspection of scattering particle in crystal using He-Ne laser assure that each crystal will perform well.

     

    CASTECH's general Nd:YLF production capabilities including

    • Rod sizes from 2 mm to 10 mm in diameter and from 1 mm to 150 mm in length
    • Orientation of rod axis to crystal axis <1 degree
    • Polished only or AR coated rods
    • Nd dopant concentrations between 0.4 and 1.2 at.%
    • Large rod and slab dimensions and non-standard dopant concentrations are available upon request

     

    Table 1. Basic Properties

    Chemical FormulaLiY1.0-xNdxF4
    Crystal StructureTetragonal
    Space GroupI41/a
    Nd (at/cm3)1.40 × 1020 at/cm3 for 1% Nd doping
    Modulus of Elasticity85 GPa
    Lattice Parametera = 5.16 Å, c = 10.85 Å 
    Melting Point819℃
    Mohs Hardness4~5 Mohs
    Density3.99 g/cm3
    Thermal Conductivity 0.063 W/cm/K
    Specific Heat 0.79 J/g/K
    Thermal Expansion Coefficient8.3 × 10-6 /K∥c, 13.3×10-6 /K⊥c

     

     Table 2. Optical Properties

    Transparency Range180-6700 nm
    Peak Stimulated Emission Cross Section

    1.8 × 10-19 /cm2 (E∥c) at 1047 nm

    1.2 × 10-19 /cm2  (E⊥c) at 1053 nm

    Fluorescence Lifetime 485 µs for 1% Nd doping
    Scatter Losses<0.2% /cm

    Peak Absorption Coefficient

     (for 1.2% Nd)

    α = 10.8 cm-1 (792.0 nm E∥c)

    α = 3.59 cm-1 (797.0 nm E⊥c)

    Laser Wavelength

    1047 nm (∥c, a-cut crystal)

    1053 nm (⊥c, a or c-cut crystal)

    Sellmeier Equations (λ in µm):

    no2 = 1.38757 + 0.70757λ2 / (λ2 - 0.00931) + 0.18849λ2 / (λ2 - 50.99741)

    ne2 = 1.31021 + 0.84903λ2 / (λ2 - 0.00876) + 0.53607λ2 / (λ2 - 134.9566)

     

    Table 3. Index of Refraction

    Wavelength (nm)none
    2621.4851.511
    3501.4731.491
    5251.4561.479
    10501.4481.47
    20651.4421.464

     

    Table 4. dn / dT

    Wavelength (nm)E // cE ⊥ c
    436-2.44 × 10-6/℃-0.54 × 10-6/℃
    578-2.86 × 10-6/℃-0.91 × 10-6/℃
    1060-4.30 × 10-6/℃-2.00 × 10-6/℃

     

    Specifications of Nd:YLF crystal from CASTECH

    Table 5. Specifications

    Standard Dopant ConcentrationNd: 1.1 ± 0.1%
    Surface quality (scratch/dig)10/5 to MIL-PRF-13830B
    Wavefront Distortion≦λ/4 @633 nm
    Surface Flatnessλ/8 @633 nm
    Parallelism20 arc sec
    Perpendicularity≦15 arc min
    Chamfer≦0.2 mm × 45°
    End CoatingR<0.15% @1047/1053 nm

     

    Key words:
    • laser crystal
    • Nd:YLF rod
    • Czochralski method
    • Nd-doped laser-active material

Inquiry List

Submit